Place of Origin:
China
Brand Name:
JBHD
Certification:
CE、ISO、SGS
Model Number:
1100
Contact Us
Product Description
It is used to make some structural parts with specific properties, with the characteristics of high plasticity, corrosion resistance, good conductivity and thermal conductivity.
1100 is industrial pure aluminum, the aluminum content (mass fraction) is 99.00%, and it can not be strengthened by heat treatment. It has high corrosion resistance, electrical conductivity and thermal conductivity, low density and good plasticity. It can produce all kinds of aluminum materials by pressure processing, but low strength. Other process properties are basically the same as 1050A. 1100 is usually used to require good formability, high corrosion resistance and no need for high strength, such as food and chemical handling and storage equipment, sheet metal products, hollow hardware processed by drawing goods spinning, welding combination keys, reflectors, nameplates, etc.
Description of application effect
Products Name | Cold treatment industrial aluminum bars or 5456 3003 6063 Aluminum alloy |
Material | Aluminum |
Other Material | 1060, 1050, 1070, 1100, 3003, 3004, 5052, 5652, 5154, 5254, 5454, 5083, 5086, 5056, 5456, 2024, 2014, 6061, 6063 ,etc |
Standard | ASTM, SUS, DIN etc |
Surface | Bright, polished, hair line, brush, embossed, etc |
Payment Term | L/C , D/A , D/P , T/T , West Union , Money Gram , other |
Price Term | FOB, CIF, CFR , CNF etc |
Package | Export standard package:bundled wooden box or be required; The inner size of container is below: (1) 20 foot GP:5.8m(length)x2.13m(width)x2.18m(high)about24-26 CBM (2) 40 foot GP:11.8m(length)x2.13m(width)x2.72m(high)about68 CBM |
Delievery Time | 5-15days |
Loading Port | china |
Supply Ability | 3000 tons per yaer |
Alloy | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | OTHERS | OTHERS | Al |
1050 | 0.25 | 0.4 | 0.05 | 0.05 | 0.05 | — | 0.05 | 0.03 | 0.03 | — | 99.5 |
1070 | 0.2 | 0.25 | 0.04 | 0.03 | 0.03 | — | 0.04 | 0.03 | 0.03 | — | 99.7 |
1100 | 0.95 Si + Fe | 0.05-0.20 | 0.05 | — | — | 0.1 | — | 0.05 | 0.15 | 99 | |
2024 | 0.5 | 0.5 | 3.8-4.9 | 0.30-0.9 | 1.2-1.8 | 0.1 | 0.25 | 0.15 | 0.05 | 0.15 | Rem. |
3003 | 0.6 | 0.7 | 0.05-0.20 | 1.0-1.5 | — | — | 0.1 | — | 0.05 | 0.15 | Rem. |
3004 | 0.3 | 0.7 | 0.25 | 1.0-1.5 | 0.8-1.3 | — | 0.25 | — | 0.05 | 0.15 | Rem. |
3005 | 0.6 | 0.7 | 0.3 | 1.0-1.5 | 0.20-0.6 | 0.1 | 0.25 | 0.1 | 0.05 | 0.15 | Rem. |
5005 | 0.3 | 0.7 | 0.2 | 0.2 | 0.50-1.1 | 0.1 | 0.25 | — | 0.05 | 0.15 | Rem. |
5052 | 0.25 | 0.4 | 0.1 | 0.1 | 2.2-2.8 | 0.15-0.35 | 0.1 | — | 0.05 | 0.15 | Rem. |
5252 | 0.08 | 0.1 | 0.1 | 0.1 | 2.2-2.8 | — | 0.05 | — | 0.03 | 0.1 | Rem. |
6061 | 0.40-0.8 | 0.7 | 0.15-0.40 | 0.15 | 0.8-1.2 | 0.04-0.35 | 0.25 | 0.15 | 0.05 | 0.15 | Rem. |
7075 | 0.4 | 0.5 | 1.2-2.0 | 0.3 | 2.1-2.9 | 0.18-0.28 | 5.1-6.1 | 0.2 | 0.05 | 0.15 | Rem. |
Alloy | Temper | Tensile Strength | Yield Strength | Elongation (%) | Tensile Strength | Yield Strength | |
(ksi) | (ksi) | 0.01-0.05 in | 0.051-0.125 in | (MPa) | (MPa) | ||
1100 | H12 | 16 | 15 | 4 | 12 | 110.3 | 103.4 |
H14 | 18 | 17 | 3 | 10 | 124.1 | 117.2 | |
3003 | H12 | 19 | 18 | 9 | 11 | 131 | 124.1 |
H14 | 22 | 21 | 3 | 7 | 151.7 | 144.8 | |
3004 | H32 | 31 | 25 | 6 | 15 | 213.7 | 172.4 |
H34 | 35 | 29 | 5 | 10 | 241.3 | 199.9 | |
3005 | H12 | 26 | 24 | 5 | 13 | 179.3 | 165.5 |
H14 | 29 | 28 | 4 | 9 | 199.9 | 193.1 | |
5005 | H12 | 20 | 19 | 5 | 9 | 137.9 | 131 |
H14 | 23 | 22 | 4 | 7 | 158.6 | 151.7 | |
5052 | H32 | 33 | 28 | 7 | 10 | 227.5 | 193.1 |
H34 | 38 | 31 | 6 | 8 | 262 | 213.7 | |
5056 | O | 42 | 22 | 23 | 24 | 289.6 | 151.7 |
H38 | 60 | 50 | 6 | 13 | 413.7 | 344.7 | |
6061 | T4 | 35 | 21 | 22 | 24 | 241.3 | 144.8 |
T6 | 45 | 40 | 12 | 17 | 310.3 | 275.8 | |
7075 | O | 33 | 15 | 16 | 18 | 227.5 | 103.4 |
T6 | 83 | 73 | 11 | 12 | 572.3 | 503. |